317L raises molybdenum to 3-4% and nickel to 11-15%, giving materially better pitting and crevice resistance than 316L in strong chloride and dilute sulphuric service — the usual step up when 316L is pitting but duplex is not wanted.

UNS: S31703 | Category: Austenitic Stainless Steel

Size Range

Outer Diameter: Thickness 3 - 80 mm · Width 1000-3000 mm · Length 2000-12000 mm

Wall Thickness: 3 - 80 mm

Chemical Composition (%)

CSiMnPSCrNiMo
0.030 max1.00 max2.00 max0.045 max0.030 max18.00-20.0011.00-15.003.00-4.00

Mechanical Properties

Yield Strength Rp0.2
205 MPa min
Tensile Strength Rm
515 MPa min
Elongation A5
40% min
Hardness
217 HB max

Applicable Standards

Applications

Industries Served

Equivalent Grades

EN
1.4438 / X2CrNiMo18-15-4
JIS
SUS 317L